Test report of bulletproof fabric – SB160 27 Layers 60 degrees

Test Sample 27 Layers SB160 UHMWPE UD (without foam at back) Test Standard GA141-2010 level 2 (compare to NIJ 0101.06 IIIA) Test Ammunition 7.62x25mm Lead Core x 6 shots Test By China Ordnance Equipment Test Center Test Time 2022.11 Test Result All passed testing (Sample Condition: 60 Degrees Temperature) Test report of bulletproof fabric SB160 27 Layers 60 degrees Distance Angle Shooting Sequence Muzzle Velocity (m/s) Penetration BFS Requirement BFS depth 5M 0 1 447 no <=25mm 25mm 5M 0 2 451 no <=25mm 23mm 5M 0 3 448 no <=25mm 21mm

Read More »

Test report of bulletproof fabric – SB160 25 Layers

Test Sample 25 Layers SB160 UHMWPE UD (without foam at back) Test Standard GA141-2010 level 2 (compare to NIJ 0101.06 IIIA) Test Ammunition 7.62x25mm Lead Core x 6 shots Test By China Ordnance Equipment Test Center Test Time 2022.11 Test Result All passed testing (Sample Condition: Normal Temperature) Test report of bulletproof fabric SB160 25 Layers Distance Angle Shooting Sequence Muzzle Velocity (m/s) Penetration BFS Requirement BFS depth 5M 0 1 453 no <=25mm 24mm 5M +30 2 442 no <=25mm 18mm 5M -45 3 449 no <=25mm 20mm 5M 0 4 454 no <=25mm 22mm 5M 0 5 454 no <=25mm 23mm 5M 0 6 448 no <=25mm 25mm

Read More »

Test report of bulletproof fabric – SB130 35 Layers -40 Degrees

Test Sample 35 Layers SB130 UHMWPE UD (without foam at back) Test Standard GA141-2010 level 2 (compare to NIJ 0101.06 IIIA) Test Ammunition 7.62x25mm Lead Core x 6 shots Test By China Ordnance Equipment Test Center Test Time 2022.11 Test Result All passed testing (Sample Condition: After -40 Degrees Temperature) Test report of bulletproof fabric SB130 35 Layers -40 Degrees Distance Angle Shooting Sequence Muzzle Velocity (m/s) Penetration BFS Requirement BFS depth 5M 0 1 443 no <=25mm 24mm 5M 0 2 452 no <=25mm 23mm 5M 0 3 451 no <=25mm 20mm

Read More »

Test report of bulletproof fabric – SB130 37 Layers

Test Sample 37 Layers SB130 UHMWPE UD (without foam at back) Test Standard GA141-2010 level 2 (compare to NIJ 0101.06 IIIA) Test Ammunition 7.62x25mm Lead Core x 6 shots Test By China Ordnance Equipment Test Center Test Time 2022.9 Test Result All passed testing (Sample Condition: Normal Temperature) Test report of bulletproof fabric SB130 37 Layers Distance Angle Shooting Sequence Muzzle Velocity (m/s) Penetration BFS Requirement BFS depth 5M 0 1 443 no <=25mm 18mm 5M +30 2 443 no <=25mm 19mm 5M -45 3 444 no <=25mm 21mm 5M 0 4 452 no <=25mm 21mm 5M 0 5 448 no <=25mm 20mm 5M 0 6 447 no <=25mm 21mm

Read More »

Test report of bulletproof fabric – SB130 35 Layers

Test Sample 35 Layers SB130 UHMWPE UD (without foam at back) Test Standard GA141-2010 level 2 (compare to NIJ 0101.06 IIIA) Test Ammunition 7.62x25mm Lead Core x 6 shots Test By China Ordnance Equipment Test Center Test Time 2022.10 Test Result All passed testing (Sample Condition: Normal Temperature) Test report of bulletproof fabric SB130 35 Layers Distance Angle Shooting Sequence Muzzle Velocity (m/s) Penetration BFS Requirement BFS depth 5M 0 1 443 no <=25mm 19mm 5M +30 2 454 no <=25mm 21mm 5M -45 3 452 no <=25mm 22mm 5M 0 4 450 no <=25mm 21mm 5M 0 5 451 no <=25mm 24mm 5M 0 6 447 no <=25mm 22mm

Read More »
guodun armor bulletproof vest and fabric

Test report of bulletproof fabric – SB166 3kg/m2 for 9mm V50

Test Sample 3kg/m2 (13 Layers) SB166-225 UHMWPE UD Test Standard NIJ 0101.06 IIIA 9mm Test Ammunition 9mm FMJ, 124gr x 6 shots Test By China Ordnance Equipment Test Center Test Time 2021.10 Test Result V50 value 480.17m/s (Sample Condition: Normal Temperature) Test report of bulletproof fabric SB166 3kg/m2 for 9mm V50

Read More »

Test report of bulletproof fabric NIJ IIIA – SB130 38 layers

Summary of bulletproof fabric NIJ IIIA test report Test Sample 38 Layers SB130 UHMWPE UD only (without anti-trauma foam at back) Test Standard NIJ 0101.06 IIIA Test Ammunition .44 Magnum SJHP 240gr x 6 shots Test By U.S H.P white lab Test Time 2010 Test Result All passed testing for NIJ IIIA Test report of bulletproof fabric NIJ IIIA

Read More »

Test report of bulletproof fabric NIJ IIIA .357 SIG – SB130 38 layers

Summary of bulletproof fabric NIJ IIIA .357 SIG test report Test Sample 38 Layers SB130 UHMWPE UD only (without anti-trauma foam at back) Test Standard NIJ 0101.06 IIIA Test Ammunition .357 SIG TMJ 125gr x 6 shots Test By U.S H.P white lab Test Time 2010 Test Result All passed testing for NIJ IIIA Test report of bulletproof fabric NIJ IIIA .357 SIG

Read More »

Test report of bulletproof fabric NIJ II .357 Magnum – SB130 33 layers

Summary of bulletproof fabric NIJ II .357 Magnum test report Test Sample 33 Layers SB130 UHMWPE UD only (without anti-trauma foam at back) Test Standard NIJ 0101.06 II .357 Magnum Test Ammunition .357 Magnum JSP 158gr x 6 shots Test By U.S H.P white lab Test Time 2010 Test Result All passed testing for NIJ II Test report of bulletproof fabric NIJ II .357 Magnum

Read More »

Test report of bulletproof fabric NIJ II .357 Magnum

Summary of bulletproof fabric NIJ II .357 Magnum test report Test Sample 32 – 39 Layers SB130 UHMWPE UD only (without anti-trauma foam at back) Test Standard NIJ 0101.06 II .357 Magnum Test Ammunition .357 Magnum JSP 158gr x 6 shots Test By U.S H.P white lab Test Time 2009 Test Result All passed testing for NIJ II Test report of bulletproof fabric NIJ II .357 Magnum

Read More »
44magnumaftershot

Test report of bulletproof fabric – SB166 3.9kg/m2

Test Sample 3.9kg/m2 (26 Layers) SB166-150 UHMWPE UD (with 5mm anti-trauma foam at back) Test Standard GA141-2010 level 2 (a reference to NIJ 0101.06 IIIA .44magnum) Test Ammunition 7.62x25mm Lead Core x 6 shots Test By China Ordnance Equipment Test Center Test Time 2021.9 Test Result All passed testing (Sample Condition: Normal Temperature) Test report of bulletproof fabric SB166 3.9kg/m2 Distance Angle Shooting Sequence Muzzle Velocity (m/s) Penetration BFS Requirement BFS depth 5M 0 1 442 no <=25mm 21mm 5M +30 2 444 no <=25mm 23mm 5M -45 3 440 no <=25mm 8mm 5M 0 4 450 no <=25mm 11mm 5M 0 5 452 no <=25mm 13mm 5M 0 6 454 no <=25mm 20mm

Read More »

Test report of bulletproof fabric – SB166 4.5kg/m2

Test Sample 4.5kg/m2 (30 Layers) SB166 UHMWPE UD (with 5mm anti-trauma foam at back) Test Standard GA141-2010 level 3 (higher than NIJ 0101.06 IIIA) Test Ammunition 7.62x25mm Lead Core x 6 shots Test By China Ordnance Equipment Test Center Test Time 2021.2 Test Result All passed testing (Sample Condition: Normal Temperature) Test report of bulletproof fabric SB166 4.5kg/m2 Distance Angle Shooting Sequence Muzzle Velocity (m/s) Penetration BFS Requirement BFS depth 5M 0 1 512 no <=25mm 14mm 5M +30 2 508 no <=25mm 12mm 5M -45 3 505 no <=25mm 12mm 5M 0 4 507 no <=25mm 15mm 5M 0 5 509 no <=25mm 14mm 5M 0 6 505 no <=25mm 11mm

Read More »